S. S. KHARDEKAR INDIA PVT. LTD.
When Slag Coagulant comes in contact with the metal, it reacts with the slag & starts coagulation i.e. formation of spongy agglomeration. The Coagulation depends on Expansion of Granules.
Cr2O3: 45-47%, SiO2: 1% Max., Fe2O3: 27-29%, Al2O3: 14.5%, CaO: 0.18 typical, Max 0.2%,
MgO: 10.2 Typical & max. 11%, TiO2: 0.69%, V2O5: 0.34%, P: 0.0029%, S: 0.0029%, Cr:Fe ratio: 1.58:1
Bulk density: 155-165 lbs/cu.ft
AFS No.: 40-50